Second National Conference On “Energy Efficient Mechanical System Design And Manufacturing” EMSDM-2015, PSG college of Technology, Coimbatore, India (2015)

Cite this Research Publication

Dr. M. Ramu, M. Bharat, and V Prabhu Raja, “Effect of Weld Defects on the Fatigue Life of the Ring Specimen”, Second National Conference On “Energy Efficient Mechanical System Design And Manufacturing” EMSDM-2015. PSG college of Technology, Coimbatore, India, 2015.