Publication Type : Conference Proceedings
Publisher : International symbosium on joining of materials
Source : International symbosium on joining of materials, WRI, Trichy (2012)
Campus : Coimbatore
School : School of Engineering
Department : Mechanical Engineering
Year : 2012
Abstract :
Cite this Research Publication : S. Quadir Moinuddin, .K, R., Dr. Saimurugan M., Santhakumari, A., and Rajasekaran, N., “Signature Analysis of welding defects in STB joints using GMAW process”, International symbosium on joining of materials. WRI, Trichy, 2012.